=The Scanning Electron Microscopes at Danchip = | |||
At the moment we have three SEM's. Together they cover a wide range of needs in the cleanroom: From the fast in-process verification of different process parameters such as etch rates, step coverages or lift-off quality to the ultra high resolution images on any type of sample intended for publication. | At the moment we have three SEM's. Together they cover a wide range of needs in the cleanroom: From the fast in-process verification of different process parameters such as etch rates, step coverages or lift-off quality to the ultra high resolution images on any type of sample intended for publication. | ||
Revision as of 17:39, 24 November 2007
The Scanning Electron Microscopes at Danchip
At the moment we have three SEM's. Together they cover a wide range of needs in the cleanroom: From the fast in-process verification of different process parameters such as etch rates, step coverages or lift-off quality to the ultra high resolution images on any type of sample intended for publication.
The SEM that will cover most users needs is the Leo SEM. It is a very reliable and rugged field emission instrument that provides high quality images of most samples. Due to its robustness new users only need a mandatory two hour training session before they are free to use it by themselves.