Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/nano/Sinano35: Difference between revisions
Appearance
Created page with "== The Sinano3.5 recipe == {| border="2" cellpadding="2" cellspacing="1" |+ '''Recipe Sinano3.5''' |- ! rowspan="6" align="center"| Recipe | Gas | BCl<sub>3</sub> 5 sccm, HB..." |
|||
| Line 31: | Line 31: | ||
|- | |- | ||
| Mask | | Mask | ||
| 180 nm zep etched down to 43 nm | | The [[Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/nano/nanoetch/180nmzep|180 nm zep resist]] etched down to 43 nm | ||
|- | |- | ||
|} | |} | ||