Specific Process Knowledge/Thermal Process/BCB Curing Oven: Difference between revisions
Appearance
| Line 32: | Line 32: | ||
|style="background:LightGrey; color:black"|Temperature | |style="background:LightGrey; color:black"|Temperature | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
* | *22 - 450<sup>o</sup>C | ||
|- | |- | ||
|style="background:LightGrey; color:black"|Nitrogen flows | |style="background:LightGrey; color:black"|Nitrogen flows | ||
Revision as of 11:16, 3 December 2012
BCB Curing Oven
The BCB Curing Oven is mainly used for curing of BCB (bisbenzocyclobutene) and for alloying of metals in a nitrogen atmosphere.
During processing the furnace is rapidly heated by use of five halogen lamps situated below the sample. The furnace is purged with a high or a low nitrogen flow. Samples are processed at atmospheric pressure or at vacuum.
The user manual, user APV, technical information and contact information can be found in LabManager:

Process information
There are no standard processes on the furnace.
| Equipment | BCB Curing Oven | |
|---|---|---|
| Purpose |
| |
| Process parameter range | Temperature |
|
| Nitrogen flows |
| |
| Pressure |
| |
| Substrates
(Remember to use the right carrier wafer) |
Batch size |
|
| Allowed materials |
| |