Revision as of 14:57, 30 November 2012
Deposition of Titanium Oxide
Titanium oxide can be deposited only by sputter technique. At the moment the only system where we have a target for Titanium oxide is IBE/IBSD Ionfab300. The target is Ti. During the sputter deposition oxygen is added to the chamber resulting in Titanium oxide on the sample.
Comparison of the methods for deposition of Titanium Oxide
| Sputter technique using IBE/IBSD Ionfab300 | Sputter technique Lesker | |
|---|---|---|
| Stoichiometry |
|
|
| Film thickness |
|
|
| Deposition rate |
|
|
| Process Temperature |
|
|
| Step coverage |
|
|
| Film quality |
|
|
| Batch size |
|
|
| Material allowed |
|
|
| More process info on TiO2 |
|