| Line 15: | Line 15: | ||
==Process parameters for the two standard deposition recipes on the TEOS furnace:== | ==Process parameters for the two standard deposition recipes on the TEOS furnace:== | ||
{| border="2" cellspacing="1" cellpadding=" | {| border="2" cellspacing="1" cellpadding="0" | ||
!Recipe name | !Recipe name | ||
!Wafer size and number of wafers | !Wafer size and number of wafers | ||