A3 Furnace phosphorus drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide and drive-in of phosphor after a pre-deposition. Phospher pre-deposition takes place in the A4 Furnace phosphorus pre-dep. A3 can also be used for drive in of phosphor which has been ion implanted.  
The A3 Furnace Phosphor drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide and drive-in of phosphorus after a pre-deposition. Phosphorus pre-deposition takes place in the A4 Furnace Phosphor pre-dep. The A3 furnace can also be used for drive-in of phosphorus which has been ion implanted.  


A3 is the third furnace tube in the A-stack positioned in cleanroom 2. The A-stack together with furnace C2 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the [http://www.labmanager.danchip.dtu.dk/view_binary.php?fileId=1250 cross contamination chart]. If you are in doubt, please send a mail to [mailto:furnace@danchip.dtu.dk the Furnace group].
A3 is the third furnace tube in the A-stack positioned in cleanroom 2. The A-stack together with the C2 Furnace Gate oxide are the cleanest of all furnaces in the cleanroom. Please be aware of which substrates are allowed to enter this furnace. Check the [http://www.labmanager.danchip.dtu.dk/view_binary.php?fileId=1250 cross contamination chart].




'''The user manual(s), quality control procedure(s) and results, technical information and contact information can be found in LabManager:'''
'''The user manual, quality control procedure and results, technical information and contact information can be found in LabManager:'''


'''[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=82 Phosphor Drive-in]'''
'''[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=82 Furnace A3: Phosphor Drive-in]'''


==Process knowledge==
==Process knowledge==

Revision as of 09:54, 29 November 2012

A3 Furnace Phosphorus drive-in

A3 phosphorus drive-in furnace: positioned in cleanroom 2

The A3 Furnace Phosphor drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide and drive-in of phosphorus after a pre-deposition. Phosphorus pre-deposition takes place in the A4 Furnace Phosphor pre-dep. The A3 furnace can also be used for drive-in of phosphorus which has been ion implanted.

A3 is the third furnace tube in the A-stack positioned in cleanroom 2. The A-stack together with the C2 Furnace Gate oxide are the cleanest of all furnaces in the cleanroom. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart.


The user manual, quality control procedure and results, technical information and contact information can be found in LabManager:

Furnace A3: Phosphor Drive-in

Process knowledge

Overview of the performance of the phosphorus drive-in furnace and some process related parameters

Purpose Drive-in of phosphor, oxidation of silicon and annealing of the oxide. Oxidation:
  • Dry
  • Wet: with torch (H2+O2)
Performance Film thickness
  • Dry SiO2: 50 Å to ~2000 Å (takes too long to make it thicker)
  • Wet SiO2: 50 Å to ~3 µm (takes too long to make it thicker)
Process parameter range Process Temperature
  • 800-1150 oC
Process pressure
  • 1 atm
Gasses on the system
  • O2, N2 and H2
Substrates Batch size
  • 1-30 4" wafer (or 2" wafers) per run
Substrate material allowed