Specific Process Knowledge/Thermal Process/A4 Phosphor Pre-dep furnace: Difference between revisions

From LabAdviser
Mdyma (talk | contribs)
Mdyma (talk | contribs)
Line 2: Line 2:
[[Image:C4helstak.jpg|thumb|300x300px|A1 Boron drive in furnace: positioned in cleanroom 2]]
[[Image:C4helstak.jpg|thumb|300x300px|A1 Boron drive in furnace: positioned in cleanroom 2]]


A4 is a furnace to dope Si wafers with Phosphor to make conductive lanes, etch stops etc. The doping source is Phosphoryl chloride (commonly called phosphorus oxychloride) is a colourless liquid with the formula POCL3.
A4 is a furnace to dope Si wafers with Phosphor to make conductive lanes, etch stops etc. The doping source is Phosphoryl chloride (commonly called phosphorus oxychloride) is a colourless liquid with the formula POCl<sub>3</sub>.


A4 is the lowest furnace tube in the A-stack positioned in cleanroom 2. The A-stack together with furnace C2 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart. If you are in doubt, please ask one from the furnace team.
A4 is the lowest furnace tube in the A-stack positioned in cleanroom 2. The A-stack together with furnace C2 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the [http://www.labmanager.danchip.dtu.dk/view_binary.php?fileId=1250 cross contamination chart]. If you are in doubt, please send a mail to [mailto:furnace@danchip.dtu.dk furnace@danchip.dtu.dk].


==Overview of the performance of the Phosphor pre-dep furnace and some process related parameters==
==Overview of the performance of the Phosphor pre-dep furnace and some process related parameters==

Revision as of 13:56, 26 November 2012

A4 Furnace Phosphor pre-dep

A1 Boron drive in furnace: positioned in cleanroom 2

A4 is a furnace to dope Si wafers with Phosphor to make conductive lanes, etch stops etc. The doping source is Phosphoryl chloride (commonly called phosphorus oxychloride) is a colourless liquid with the formula POCl3.

A4 is the lowest furnace tube in the A-stack positioned in cleanroom 2. The A-stack together with furnace C2 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart. If you are in doubt, please send a mail to furnace@danchip.dtu.dk.

Overview of the performance of the Phosphor pre-dep furnace and some process related parameters

Purpose Doping of Phosphor
Performance
Process parameter range Process Temperature
  • 900-1150 oC
Process pressure
  • 1 atm
Gasses on the system
  • POCL3
Substrates Batch size
  • 1-30 4" wafer (or 2" wafers) per run
Substrate material allowed
  • Silicon wafers (new from the box or RCA cleaned)
  • In doubt: look at the cross contamination sheet or ask one from the furnace team
Material NOT allowed
  • wafers must NOT have been exposed to metal prior to A4
  • wafers must NOT have been stored in dirty boxes (i.e. boxes that has contained wafers with metal)