A1 Furnace boron drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide, drive-in of boron after a predeposition, oxidation of the boron phase layer. Boron predeposition takes place in the A2 Furnace boron pre-dep. It can also be used for drive in of boron which has been ion implanted. | A1 Furnace boron drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide, drive-in of boron after a predeposition, oxidation of the boron phase layer. Boron predeposition takes place in the A2 Furnace boron pre-dep. It can also be used for drive in of boron which has been ion implanted. | ||
A1 is the top furnace tube in the A-stack positioned in cleanroom 2. The A-stack together with furnace C2 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check [http://www.labmanager.danchip.dtu.dk/view_binary.php?fileId=1250 the cross contamination chart]. If you are in doubt, please send a mail to [mailto:furnace@danchip.dtu.dk | A1 is the top furnace tube in the A-stack positioned in cleanroom 2. The A-stack together with furnace C2 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check [http://www.labmanager.danchip.dtu.dk/view_binary.php?fileId=1250 the cross contamination chart]. If you are in doubt, please send a mail to [mailto:furnace@danchip.dtu.dk furnace@danchip.dtu.dk]. | ||
'''The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:''' | '''The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:''' | ||