== Wafer Information ==
== Wafer Information ==
DTU Danchip has a stock of most used silicon and glass wafers; most of these wafers are to be found in stock in cleanroom 2. Whenever you take a wafer from stock, you should buy the wafer from the [http://labmanager.danchip.dtu.dk/function.php?module=Wafer&view=list&page_id=16| wafer shop] in LabManager. The Price can also be found in the wafer shop.  
DTU Danchip has a stock of silicon and glass wafers; the most used of these wafers are located on the wafershelves in cleanroom 2. Whenever you take a wafer from stock, you should buy the wafer from the [http://labmanager.danchip.dtu.dk/function.php?module=Wafer&view=list&page_id=16| wafer shop] in LabManager. The Price can also be found in the wafer shop.  


The waferbox name consists of two characters and three to four numbers, eg OP337, according to the code below:
The waferbox name consists of two characters and three to four numbers, eg OP337, according to the code below:

Revision as of 16:01, 8 January 2013

Wafer Information

DTU Danchip has a stock of silicon and glass wafers; the most used of these wafers are located on the wafershelves in cleanroom 2. Whenever you take a wafer from stock, you should buy the wafer from the wafer shop in LabManager. The Price can also be found in the wafer shop.

The waferbox name consists of two characters and three to four numbers, eg OP337, according to the code below:

Origin of waferbox names
O P 337
Indicates the company where the wafers are bought Type of doping in the wafer shipment number


Wafers available at DTU Danchip

Wafers available at DTU Danchip
  Shelf Size Type Thickness Resistivity
SSP (single side polished) bottom 4" N+P 525 µm 1-20 Ωcm
SSP (single side polished) top 6" N or P 625 µm 1-20 Ωcm
DSP (double side polished) middle 4" N+P 350 µm 1-20 Ωcm
wafers with different layers top 4" and 6"      
Boron glasswafers middle 4"   1 mm  


Wafer boxes and single wafer carriers

New clean wafer boxes and single wafer carriers can be found in the changing area. Ask DTU Danchip personnel for help if stock is low.

Substrate information

Substrates