Sample material: Patterned fused silica.  
Sample material: Patterned fused silica.  
Measurement: Depth of pattern
Measurement: Depth of pattern
Acceptance criteria:Depth within ±1% from a standard profiler measurement and repeatability (3 successive measurements) within 0.1%  
Acceptance criteria:Depth within ±1% from a standard profiler measurement and repeatability (3 successive measurements) within 0.1%  


Standard profiler measurement: