Specific Process Knowledge/Thin film deposition/Furnace LPCVD PolySilicon: Difference between revisions
Appearance
| Line 6: | Line 6: | ||
The LPCVD polysilicon deposition is a batch process, where polySi is deposited on a batch of 25 or 50 wafers (6" polySi furnace) or 30 wafers (4" polySi furnace). The polySi has a good step coverage, and especially for standard polySi the film thickness is very uniform over the wafers. | The LPCVD polysilicon deposition is a batch process, where polySi is deposited on a batch of 25 or 50 wafers (6" polySi furnace) or 30 wafers (4" polySi furnace). The polySi has a good step coverage, and especially for standard polySi the film thickness is very uniform over the wafers. | ||
The reactive gas is silane (SiH<sub>4</sub>). The dopant for boron doped polySi is BCl<sub>3</sub> (6" polySi furnace) or B<sub>2</sub>H<sub>6</sub> (4" polySi furnace), and for phosphorous doped polySi the dopant is PH<sub>3</sub>. For standard polysilion the deposition takes place at a temperature of 620<sup>o</sup>C and a pressure of 200-250 | The reactive gas is silane (SiH<sub>4</sub>). The dopant for boron doped polySi is BCl<sub>3</sub> (6" polySi furnace) or B<sub>2</sub>H<sub>6</sub> (4" polySi furnace), and for phosphorous doped polySi the dopant is PH<sub>3</sub>. For standard polysilion the deposition takes place at a temperature of 620<sup>o</sup>C and a pressure of 200-250 mTorr. For amorphous polysilicon the deposition temperatures and thus the deposition rate are lower, and for boron and phosphorous doped polySi the deposition temperature is 600<sup>o</sup>C - 620<sup>o</sup>C depending on whether you use the 6" or the 4" polySi furnace. For phousphorous doped polySi the deposition rate is approximately ten times lower than for boron doped polySi. More process information about the process parameters can be found in the table below. | ||
To get information on how to operate the furnaces please read the user manuals which are uploaded to the machine pages in LabManager or consult the Furnace group at Danchip (furnace@danchip.dtu.dk). | To get information on how to operate the furnaces please read the user manuals which are uploaded to the machine pages in LabManager or consult the Furnace group at Danchip (furnace@danchip.dtu.dk). | ||