Specific Process Knowledge/Etch/ICP Metal Etcher: Difference between revisions
Appearance
| Line 6: | Line 6: | ||
* titanium tungsten | * titanium tungsten | ||
* chromium | * chromium | ||
Over time it is our intention to add other materials to the list such as molybdenum, tungsten | Over time it is our intention to add other materials to the list such as molybdenum, tungsten, titaniumoxides or piezo-materials such as ZnO. However, currently you are not even allowed to expose other metals to the plasma. To etch other metals use the [[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE/IBSD Ionfab 300]]. | ||
== Recipes on the Metal Etcher == | == Recipes on the Metal Etcher == | ||