Specific Process Knowledge/Polymer Processing/Coating/Inkjet Printer: Difference between revisions
No edit summary |
|||
| Line 1: | Line 1: | ||
''The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.'' | ''The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.'' | ||
'''Feedback | '''Feedback on this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Polymer_Processing/Inkjet_printer click here]''' | ||
=Inkjet printer= | =Inkjet printer= | ||
[[File:Inkjet printer.jpg|400px|right|Inkjet printer is located in PolyFabLab, building 347.]] | [[File:Inkjet printer.jpg|400px|right|Inkjet printer is located in PolyFabLab, building 347.]]The inkjet printer is an Autodrop Gantry II printing system bought in 2020 and installed in PolyFabLab in 2025. It is a modular XYZ positioning platform for contact-less, piezo-driven inkjet dispensing. It drives interchangeable dispenser heads, Autopipettes, or piezo valves rather than a single fixed printhead, and is intended for precision deposition of inks, polymers, and other functional fluids on chips, wafers, and other flat substrates — for process development, prototyping, and small-batch work rather than high-throughput production. | ||
The user manual and contact information for the inkjet printer can be found on LabManager [https://labmanager.dtu.dk/function.php?module=Machine&view=view&page_id=169] - <nowiki>'''</nowiki>requires login<nowiki>'''</nowiki> | |||
Revision as of 11:28, 18 September 2026
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback on this page: click here
Inkjet printer

The inkjet printer is an Autodrop Gantry II printing system bought in 2020 and installed in PolyFabLab in 2025. It is a modular XYZ positioning platform for contact-less, piezo-driven inkjet dispensing. It drives interchangeable dispenser heads, Autopipettes, or piezo valves rather than a single fixed printhead, and is intended for precision deposition of inks, polymers, and other functional fluids on chips, wafers, and other flat substrates — for process development, prototyping, and small-batch work rather than high-throughput production.
The user manual and contact information for the inkjet printer can be found on LabManager [1] - '''requires login'''