Jump to content

Specific Process Knowledge/Polymer Processing/Plasma Cleaners: Difference between revisions

Bghe (talk | contribs)
Created page with "''The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.'' '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Polymer_Processing/Polymer_Processing_Plasma_Cleaners click here]''' =Plasma cleaner: 2 & 3= File:Plasma cleaner.jpg|400px|right|Plasma Cleaner: 2 is located in PolyFabLab,..."
 
Meenadh (talk | contribs)
Line 7: Line 7:
[[File:Plasma cleaner.jpg|400px|right|Plasma Cleaner: 2 is located in PolyFabLab, and Plasma Cleaner: 3 is located in the PDMS lab in building 347.]]
[[File:Plasma cleaner.jpg|400px|right|Plasma Cleaner: 2 is located in PolyFabLab, and Plasma Cleaner: 3 is located in the PDMS lab in building 347.]]


'''Tool description'''<br>
'''Plasma cleaner 2 (located in PolyFaLab) and Plasma cleaner 3 (located in PDMS lab) are Diener Atto (PC control, 13.56 MHz RF) systems installed in 2026.''' <br>