1. Non-cured PDMS: All mixtures of PDMS resin and curing agent are prepared on this area. Cellophan film is provided and must be placed on the table ALWAYS when working with uncured PDMS. | 1. Non-cured PDMS: All mixtures of PDMS resin and curing agent are prepared on this area. Cellophan film is provided and must be placed on the table ALWAYS when working with uncured PDMS. A high precision scale, a vacuum desiccator and an oven are available in this area. | ||
2. Cured PDMS: Only cured PDMS can be handled in this area. | 2. Cured PDMS: Only cured PDMS can be handled in this area. | ||