Clean well the place before leaving. Dispose all cellophane liner used. Be sure no residues of PDMS are left in the work areas, and place all PDMS residues in the C-waste container. | Clean well the place before leaving. Dispose all cellophane liner used. Be sure no residues of PDMS are left in the work areas, and place all PDMS residues in the C-waste container. | ||
[[File:PDMS through-hole methods.jpg| | [[File:PDMS through-hole methods.jpg|800px|thumb|left|Scanning Electron Microscopy (SEM) micrographs for comparison of methods to fabricate through-holes in PDMS ]] | ||
'''Laser ablation''' | '''Laser ablation''' | ||