Specific Process Knowledge/Back-end processing/PDMS Microfluidic: Difference between revisions

Cchvi (talk | contribs)
Cchvi (talk | contribs)
Line 78: Line 78:
[[File:Contact Angle Plasma Tretament vs Time.jpg|1000px|thumb|center|Pictures of contact angle for water drop on PDMS and borosilicate glass after plasma treatment in the PDMS lab at DTU for different time]]
[[File:Contact Angle Plasma Tretament vs Time.jpg|1000px|thumb|center|Pictures of contact angle for water drop on PDMS and borosilicate glass after plasma treatment in the PDMS lab at DTU for different time]]


 
[[File:Press for bonding PDMS microfluidics.jpg|thumb|Press used to improve the bonding of PDMS and glass in a microfluidic device]]


'''PDMS/PMMA bonding'''
'''PDMS/PMMA bonding'''