Specific Process Knowledge/Back-end processing/PDMS Microfluidic: Difference between revisions
| Line 47: | Line 47: | ||
The PDMS can cure without heating in ~24 hours. Curing the PDMS at higher temperatures in the oven can decrease the time spent curing. The temperatures between 60°C to 100°C can be used, and the choice must be optimized for the specific device design, and the desired mechanical and surface properties. The curing time depends on the temperature and the thickness of PDMS. As a standard procedure to cure PDMS, place the casted PDMS on the mold in the oven for at least 2 hours at ~80°C. | The PDMS can cure without heating in ~24 hours. Curing the PDMS at higher temperatures in the oven can decrease the time spent curing. The temperatures between 60°C to 100°C can be used, and the choice must be optimized for the specific device design, and the desired mechanical and surface properties. The curing time depends on the temperature and the thickness of PDMS. As a standard procedure to cure PDMS, place the casted PDMS on the mold in the oven for at least 2 hours at ~80°C. | ||
'''Demolding''' | '''Demolding''' | ||
Revision as of 14:43, 16 July 2026
THIS PAGE IS UNDER CONSTRUCTION
Unless otherwise stated, all content on this page was created by Claudia Chaves Villarreal, DTU Nanolab
Feedback to this page: click here
PDMS Lab at DTU Nanolab
Polydimethylsiloxane (PDMS), also known as silicone, has become a fundamental material for fabricating microfluidic devices with applications in health, chemistry, biomedical sciences and more.
DTU Nanolab has a dedicated laboratory for the processing of PDMS and fabrication of microfluidics located in building 347. The PDMS Lab is part of the PolyFabLab and has been equipped with brand-new instruments funded by the Novo Nordisk Foundation, alongside selected equipment and processes from previous facilities.
The laboratory has 4 different areas:
1. Non-cured PDMS: All mixtures of PDMS resin and curing agent are prepared on this area. Cellophan film is provided and must be placed on the table ALWAYS when working with uncured PDMS.
2. Cured PDMS: Only cured PDMS can be handled in this area.
3. Fume hood: safe area for handling volatile chemicals that are hazardous for human and environment health. The spin-coating machine and the hazardous waste are also located in this area.
4. Plasma machine: equipment to condition the surfaces for bonding of parts in microfluidic devices.
5. Storage area: to store chemicals, samples, sample holders, tools, and materials.
6. Personal protective equipment and emergency shower equipment: googles, lab coats, emergency shower and eyewasher are provided for the safety of lab users
Material requirements
Process flow
Mixing PDMS resin and degassing
Soft lithography micro molding
Mold surface conditioning
Molding by pouring
Molding by spin coating
Baking – Curing

The PDMS can cure without heating in ~24 hours. Curing the PDMS at higher temperatures in the oven can decrease the time spent curing. The temperatures between 60°C to 100°C can be used, and the choice must be optimized for the specific device design, and the desired mechanical and surface properties. The curing time depends on the temperature and the thickness of PDMS. As a standard procedure to cure PDMS, place the casted PDMS on the mold in the oven for at least 2 hours at ~80°C.
Demolding
After curing, the PDMS microfluidic chip is a solid and chemically inert material. Once cooled, the PDMS is easily peeled off from the mold. The demolding and further processes of cured PDMS must be done in the designated “cured PDMS”. If the demolding does not occur readily, wetting it with isopropanol or ethanol might be helpful. Otherwise, the mold must be conditioned properly before casting the PDMS.
3D printing
Cutting PDMS

Punching
Create access ports, also known as through-holes, using manual commercial punchers available for biopsy or general use. Punch the devices on top of the green cutting board to extend the lifetime of the puncher blade and to avoid marking the table. Solvents like ethanol, isopropanol and acetone can be used as lubricants to facilitate the cutting and result in a cleaner surface. Clean well the place before leaving. Dispose all cellophane liner used. Be sure no residues of PDMS are left in the work areas, and place all PDMS residues in the C-waste container.

Laser ablation
Machining/milling
Air/water jet machining
Bonding
PDMS/PDMS and PDMS/glass bonding
PDMS/PMMA bonding
References
For further information contact Stephan Sylvest Keller suke@dtu.dk or Claudia Chaves Villarreal cchvi@dtu.dk