Polydimethylsiloxane (PDMS), also known as silicone, has become a fundamental material for fabricating microfluidic devices with applications in health, chemistry, biomedical sciences and more. | Polydimethylsiloxane (PDMS), also known as silicone, has become a fundamental material for fabricating microfluidic devices with applications in health, chemistry, biomedical sciences and more. | ||
DTU Nanolab has a dedicated laboratory for the processing of PDMS and fabrication of microfluidics located in building 347. The PDMS Lab is part of the PolyFabLab and has been equipped with brand-new instruments funded by the Novo Nordisk Foundation, alongside selected equipment and processes from previous facilities. | DTU Nanolab has a dedicated laboratory for the processing of PDMS and fabrication of microfluidics located in building 347. The PDMS Lab is part of the PolyFabLab and has been equipped with brand-new instruments funded by the Novo Nordisk Foundation, alongside selected equipment and processes from previous facilities. | ||
The laboratory has 4 different areas: | |||
1. Non-cured PDMS: All mixtures of PDMS resin and curing agent are prepared on this area. Cellophan film is provided and must be placed on the table ALWAYS when working with uncured PDMS. | |||
2. Cured PDMS: Only cured PDMS can be handled in this area. | |||
3. Fume hood: safe area for handling volatile chemicals that are hazardous for human and environment health. The spin-coating machine and the hazardous waste are also located in this area. | |||
4. Plasma machine: equipment to condition the surfaces for bonding of parts in microfluidic devices | |||
5. Storage area: to store chemicals, samples, sample holders, tools, and materials | |||
6. Personal protective equipment and emergency shower equipment: googles, lab coats, [https://www.inside.dtu.dk/en/work-environment/physical-work-environment/laboratorier-og-vaerksteder/oejenskylleflasker-og-noedbrusere emergency shower and eyewasher] are provided for the safety of lab users | |||
==Material requirements== | ==Material requirements== | ||
Revision as of 13:59, 16 July 2026
THIS PAGE IS UNDER CONSTRUCTION
Unless otherwise stated, all content on this page was created by Claudia Chaves Villarreal, DTU Nanolab
Feedback to this page: click here
PDMS Lab at DTU Nanolab
Polydimethylsiloxane (PDMS), also known as silicone, has become a fundamental material for fabricating microfluidic devices with applications in health, chemistry, biomedical sciences and more.
DTU Nanolab has a dedicated laboratory for the processing of PDMS and fabrication of microfluidics located in building 347. The PDMS Lab is part of the PolyFabLab and has been equipped with brand-new instruments funded by the Novo Nordisk Foundation, alongside selected equipment and processes from previous facilities.
The laboratory has 4 different areas: 1. Non-cured PDMS: All mixtures of PDMS resin and curing agent are prepared on this area. Cellophan film is provided and must be placed on the table ALWAYS when working with uncured PDMS. 2. Cured PDMS: Only cured PDMS can be handled in this area. 3. Fume hood: safe area for handling volatile chemicals that are hazardous for human and environment health. The spin-coating machine and the hazardous waste are also located in this area. 4. Plasma machine: equipment to condition the surfaces for bonding of parts in microfluidic devices 5. Storage area: to store chemicals, samples, sample holders, tools, and materials 6. Personal protective equipment and emergency shower equipment: googles, lab coats, emergency shower and eyewasher are provided for the safety of lab users
Material requirements
Process flow
Mixing PDMS resin and degassing
Soft lithography micro molding
Mold surface conditioning
Molding by pouring
Molding by spin coating
Baking – Curing
Demolding

3D printing
Cutting PDMS
Punching
Laser ablation
Machining/milling
Air/water jet machining
Bonding
PDMS/PDMS and PDMS/glass bonding
PDMS/PMMA bonding
References