PDMS microfluidics fabrication at DTU Nanolab
Material requirements
Process flow
Mixing PDMS resin and degassing
Soft lithography micro molding
Mold surface conditioning
Molding by pouring
Molding by spin coating
Baking – Curing
Alignment – Demolding
3D printing
Cutting PDMS
Punching
Laser ablation
Machining/milling
Air/water jet machining
Bonding
PDMS/PDMS and PDMS/glass bonding
PDMS/PMMA bonding
References