| Line 109: | Line 109: | ||
*TSA microscope travel range: X ±25 mm; Y +20/-75 mm (towards the flat) | *TSA microscope travel range: X ±25 mm; Y +20/-75 mm (towards the flat) | ||
''' | |||
'''Back Side Alignment:''' | |||
*Minimum distance between BSA microscope objectives: 15 mm | *Minimum distance between BSA microscope objectives: 15 mm | ||
*Maximum distance between BSA microscope objectives: 100 mm | *Maximum distance between BSA microscope objectives: 100 mm | ||
| Line 120: | Line 121: | ||
'''Microscope field of view (W x H, splitfield):''' | '''Microscope field of view (W x H, splitfield):''' | ||
*TSA 5X | *TSA 5X: | ||
**Oculars: 1. | **Oculars: 1.3 mm x 2.6 mm (Ø2.6 mm full field) | ||
**Camera: | **Camera: 350 µm x 500 µm (700 µm x 500 µm full field) | ||
*TSA 10X | *TSA 10X: | ||
**Oculars: 0. | **Oculars: 0.6 mm x 1.3 mm (Ø1.3 mm full field) | ||
**Camera: | **Camera: 150 µm x 250 µm (350 µm x 250 µm full field) | ||
*TSA special | *TSA special: | ||
**Oculars: 0. | **Oculars: 0.55 mm x 1.1 mm (Ø1.1 mm full field) | ||
**Camera: | **Camera: 150 µm x 200 µm (300 µm x 200 µm full field) | ||
*BSA camera | *BSA camera: | ||
**Low: 1. | **Low: 1.5 mm x 2 mm (3 mm x 2 mm full field) | ||
**High: | **High: 450 µm x 650 µm (950 µm x 650 µm full field) | ||
==Quality Control (QC)== | ==Quality Control (QC)== | ||