The purpose of the QC process is to check the intensity and uniformity of the exposure light in the Aligner: MA6-2, using a UV optometer. The optometer is placed at 5 fixed positions | The purpose of the QC process is to check the intensity and uniformity of the exposure light in the Aligner: MA6-2, using a UV optometer. The optometer is placed at 5 fixed positions in the exposure area on a dedicated QC chuck, and the intensity of the light is measured. | ||
The 5 intensity measurements are then used to calculate the average intensity as well as the peak uniformity error: <math>PUE[%] = \frac{min-max}{min+max} \sdot 100</math>. | The 5 intensity measurements are then used to calculate the average intensity as well as the peak uniformity error: <math>PUE[%] = \frac{min-max}{min+max} \sdot 100</math>. | ||
| Line 142: | Line 142: | ||
'''Uniformity accept limit:'''<br> | '''Uniformity accept limit:'''<br> | ||
The uniformity should be adjusted if the uniformity error is greater than 2%. | The uniformity should be adjusted if the peak uniformity error is greater than 2%. | ||