Specific Process Knowledge/Lithography/Aligners/MAvsMLA: Difference between revisions
Appearance
| Line 282: | Line 282: | ||
====Linewidth and sidewall angle vs defocus parameter (AZ 5214E)==== | ====Linewidth and sidewall angle vs defocus parameter (AZ 5214E)==== | ||
<br clear="all" /> | <br clear="all" /> | ||
'''Result of image analysis of SEM images of 2µm triplets:''' | |||
{| cellpadding="2" style="border: 2px solid darkgray;" align="left" | |||
! width="510" | | |||
|+ | |||
|- border="0" align="center" | |||
|[[Image:5214E_Profile vs defoc.jpg|500px]] | |||
|- align="center" | |||
| Linewidth and sidewall angle vs. defocus value for 1.5µm AZ 5214E exposed in Aligner: Maskless 02 (MLA2) using dose 95mJ/cm<sup>2</sup>. <br>Blue circles: Width of 2µm line. <br>Orange Squares: Sidewall angle. | |||
|} | |||
<br clear="all" /> | |||
'''SEM images of 1.5µm AZ 5214E as a function of defocus parameter for Aligner: Maskless 02 (MLA2) using dose 95mJ/cm<sup>2</sup>:''' | '''SEM images of 1.5µm AZ 5214E as a function of defocus parameter for Aligner: Maskless 02 (MLA2) using dose 95mJ/cm<sup>2</sup>:''' | ||
{|border="1" cellspacing="0" cellpadding="3" style="text-align:left;" | {|border="1" cellspacing="0" cellpadding="3" style="text-align:left;" | ||
|- | |- | ||
| Line 314: | Line 331: | ||
|[[Image:W33 MLA2 5214 F5 D95_02.jpg|280px]] | |[[Image:W33 MLA2 5214 F5 D95_02.jpg|280px]] | ||
|[[Image:W33 MLA2 5214 F12 D95_102.jpg|280px]] | |[[Image:W33 MLA2 5214 F12 D95_102.jpg|280px]] | ||
|} | |} | ||