== Nickel deposition == | |||
Nickel can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment. | Nickel can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment. | ||
Revision as of 13:57, 1 March 2013
Feedback to this page: click here
Nickel deposition
Nickel can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | E-beam evaporation (Wordentec) | |
---|---|---|
Batch size |
|
|
Pre-clean | RF Ar clean | RF Ar clean |
Layer thickness | 10Å to 1µm | 10Å to 1 µm |
Deposition rate | 2Å/s to 15Å/s | 10Å/s to 15Å/s |