Specific Process Knowledge/Lithography/Aligners/MAvsMLA: Difference between revisions
Appearance
| Line 20: | Line 20: | ||
===Resolution=== | ===Resolution=== | ||
* Table with optimal parameters and resolution for different aligners | * Table with optimal parameters and resolution for different aligners | ||
* SEM pictures | |||
<br clear="all" /> | <br clear="all" /> | ||
Revision as of 16:20, 10 June 2026
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
Mask Aligner vs Maskless Aligner
Slides presented at NNUM in Uppsala 2026: MA6 vs MLA 2026_v09
Mask design used in the investigation: LithoTestAlign_2025_v10.gds
Additional data
THIS PAGE IS UNDER CONSTRUCTION
AZ 5214E
Resolution
- Table with optimal parameters and resolution for different aligners
- SEM pictures
Yield
- Wafer maps of:
- Aligner: Maskless 02 (MLA2)
- Aligner: MA6-1
- Aligner: MA6-2 before service
- Aligner: MA6-2 after service + WEC pressure
Resist profile (sidewall angle and linewidth)
- SEM pictures to support graphs?

Blue circles: Exposed on Aligner: MA6-2 in vacuum contact.
Orange Squares: Exposed on Aligner: Maskless 02 (MLA2) using defoc 2 (QC defoc=2).

Blue circles: Exposed on Aligner: MA6-2 in vacuum contact.
Orange Squares: Exposed on Aligner: Maskless 02 (MLA2) using defoc 2 (QC defoc=2).

Blue circles: Width of 2µm line. Orange Squares: Sidewall angle.
AZ MiR 701
Resolution
- Table with optimal parameters and resolution for different aligners
Resist profile (sidewall angle and linewidth)
- SEM pictures to support graphs?

Blue circles: Exposed on Aligner: MA6-2 in vacuum contact.
Orange Squares: Exposed on Aligner: Maskless 02 (MLA2) using defoc 2 (QC defoc=2).

Blue circles: Exposed on Aligner: MA6-2 in vacuum contact.
Orange Squares: Exposed on Aligner: Maskless 02 (MLA2) using defoc 2 (QC defoc=2).

Blue circles: Width of 2µm line. Orange Squares: Sidewall angle.
AZ nLOF 2020
Resolution
- Table with optimal parameters and resolution for different aligners
Resist profile (sidewall angle and linewidth)
- SEM pictures to support graphs?

Blue circles: Exposed on Aligner: MA6-2 in vacuum contact.
Orange Squares: Exposed on Aligner: Maskless 01 (MLA1) using defoc -4 (QC defoc=-2).
Grey triangles: Exposed on Aligner: Maskless 02 (MLA2) using defoc 0 (QC defoc=2).

Blue circles: Exposed on Aligner: MA6-2 in vacuum contact.
Orange Squares: Exposed on Aligner: Maskless 01 (MLA1) using defoc -4 (QC defoc=-2).
Grey triangles: Exposed on Aligner: Maskless 02 (MLA2) using defoc 0 (QC defoc=2).

Blue circles: Width of 2µm line. Orange Squares: Sidewall angle.

Blue circles: Width of 2µm line. Orange Squares: Sidewall angle.