Line 182: Line 182:
|-
|-
|LiNbO3**||DAD321 ||B1A862 ||1-3 mm/s ||15'000 ||0.5mm
|LiNbO3**||DAD321 ||B1A862 ||1-3 mm/s ||15'000 ||0.5mm
|-
|SiC***||DAD321 ||ZP07 ||1 mm/s ||15'000 ||0.5mm
|}
|}
(*) Multiple cuts at the same location can be done if deeper cuts are needed <br>
(*) Multiple cuts at the same location can be done if deeper cuts are needed <br>
(**) Tested once 26-05-08, no systematic test done
(**) Tested once 26-05-08, no systematic test done
(***) Tested once 25-10-29, no systematic test done