Specific Process Knowledge/Lithography/Resist/UVresist/exposureDoseNaOH: Difference between revisions
Appearance
Created page with "The exposure doses listed below are for ''generic'' good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values. All doses are for standard silicon wafers, unless otherwise stated. Development is done using AZ 351B developer (NaOH) diluted 1:5. ===Aligner: MA6-1=== The Aligner: MA6-1 has an i-line..." |
No edit summary |
||
| Line 1: | Line 1: | ||
==Exposure dose for mask aligners== | |||
The exposure doses listed below are for ''generic'' good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values. | The exposure doses listed below are for ''generic'' good exposure results, and can be a compromise between getting good lines, as well as good dots, in both clear field and dark field exposures. The optimal dose for any given specific project, could be different from the listed values. | ||