Wet etching of Titanium

Wet Etch of Titanium can take place in this pp tank or in a beaker in this fume hood
We have two solutions for wet titanium etching:
- BHF
- Cold RCA1
Do it by making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. BHF etching can also take place in the PP-etch bath in the fume hood in cleanroom 2.
Comparing the two solutions
| BHF | Cold RCA1 | |
|---|---|---|
| General description | Etch of titanium with or without photoresist mask. | Etch of titanium (as stripper or with eagle resist). |
| Chemical solution | HF:NHF | NHOH:HO:HO - 1:1:5 |
| Process temperature | Room temperature | Room temperature |
| Possible masking materials |
Photoresist (1.5 µm AZ5214E) |
Eagle resist |
| Etch rate |
Not known (it bubbles while etching) |
Not known |
| Batch size |
1-5 4" in beaker 1-25 wafers at a time in PP-etch bath |
1-5 4" wafer at a time |
| Etch bath | Beaker or PP-etch bath in the fume hood in cleanroom 2. | Beaker |
| Allowed materials |
No restrictions when used in beaker or PP-etch bath in the fume hood in cleanroom 2. Make a note on the beaker of which materials have been processed. |
No restrictions when used in beaker. Make a note on the beaker of which materials have been processed. |
Dry etching of titanium
See the ICP Metal Etch page.