===Etching of TiN using ICP metal ===
===Etching of TiO2 using ICP metal has been tested Evgeniy Shkondin, DTU Nanolab===
 
Recipe used: Ti etch <br>
[[image:TiO2_etch_Evgeniy2.jpg|400px]]