TPT HB100 wire bonder comes with wires and tools and has option for mounting Gold wire (dia.: 25µm) or Aluminum wire (dia.: 33µm). write to the tool responsible person for changing wire.  
TPT HB100 wire bonder comes with wires and tools and has option for mounting Gold wire (dia.: 25µm) or Aluminum wire (dia.: 33µm). write to the tool responsible person for changing wire.  
The system has motorized Z-Y-X Axes and Bond Head Rotation. The TPT software has template of recipes allowing user to set up their own process recipe based on type of bonding and wire.   
The system has motorized Z-Y-X Axes and Bond Head Rotation. The TPT software has template of recipes allowing user to set up their own process recipe based on type of bonding and wire.   




Line 113: Line 111:
|}
|}
''For detailed information on compatible wires and bonding tools for the HB100, visit the [https://www.tpt-wirebonder.com/wires_tools/ TPT Wires & Tools] page.''
''For detailed information on compatible wires and bonding tools for the HB100, visit the [https://www.tpt-wirebonder.com/wires_tools/ TPT Wires & Tools] page.''
 
-------------------------------------
The TPT HB100 wire bonder is supplied with wires and tools, and can be configured to mount either 25 µm diameter gold wire or 33 µm diameter aluminium wire. To change the wire, please contact the tool’s responsible person.
The system features motorized Z, Y, and X axes along with bond head rotation, enabling precise and flexible operation. The integrated TPT software includes a library of recipe templates, allowing users to create and customize process recipes according to the bonding method and wire type.
===Process parameters for Gold wire (25µm)===
===Process parameters for Gold wire (25µm)===

Revision as of 10:50, 13 August 2025

Feedback to this page: click here


THIS PAGE IS UNDER CONSTRUCTION

TPT HB100 wire bonder comes with wires and tools and has option for mounting Gold wire (dia.: 25µm) or Aluminum wire (dia.: 33µm). write to the tool responsible person for changing wire. The system has motorized Z-Y-X Axes and Bond Head Rotation. The TPT software has template of recipes allowing user to set up their own process recipe based on type of bonding and wire.


HB100 Full Technical Specifications
Bonding Specifications Bonding Methods Wedge–Wedge, Ball–Wedge, Ribbon, Bump
Bond Head Capability One head for Wedge & Ball bonding (tool change only)
Wire Diameter (Gold) 12–75 µm (0.5–3 mil)
Wire Diameter (Aluminium) 17–75 µm (0.7–3 mil)
Wire & Ribbon Handling Ribbon Size Max. 25 × 250 µm (1 × 10 mil)
Wire Spool Size 2" diameter
Wire Feed Angle / Immersion Depth 90° deep access / 14 mm immersion
Ultrasonic & Bonding Parameters Ultrasonic Frequency 63.3 kHz PLL control (110 kHz option)
Ultrasonic Power 0–10 W
Bond Time 0–5 seconds
Bond Force 10–200 cN
Bonding Tool Size 1.58 mm Ø × 19 mm length (0.0624" × 0.750")
Wire Termination Bond Head Tear or Clamp Tear
Mechanics & Motion Control Z-Drive / Resolution Lead screw motor / 0.5 µm
Motorized Z Travel 100 mm (3.9")
X–Y Drive / Resolution Linear motors / 0.1 µm
Motorized X–Y Travel 100 mm (3.9")
Max. Component Width 400 mm (15.7")
Rotation Drive Accuracy ±0.5°
Control & Interface Axis Control Joystick
Screen Size 21" touchscreen
Software Environment Industrial PC with Windows
Camera & Optics Camera System Dual camera (detail + overview)
Magnification Up to 150×
View Mode Simultaneous detail & overview
Heater Stage Size 90 mm Ø surface (mechanical & vacuum clamping)
Temperature Range Up to 200 °C ±1 °C
Clamping Mechanical & vacuum

For detailed information on compatible wires and bonding tools for the HB100, visit the TPT Wires & Tools page.


The TPT HB100 wire bonder is supplied with wires and tools, and can be configured to mount either 25 µm diameter gold wire or 33 µm diameter aluminium wire. To change the wire, please contact the tool’s responsible person. The system features motorized Z, Y, and X axes along with bond head rotation, enabling precise and flexible operation. The integrated TPT software includes a library of recipe templates, allowing users to create and customize process recipes according to the bonding method and wire type.

Process parameters for Gold wire (25µm)