[[Image:section under construction.jpg|70px]] ''Is currently in building 346 Pheenex lab.''
[[Image:K-S 4524 wirebonder DTU.jpg|thumb|200px|K&S 4524 ball wire bonder]]
 
<span style="background:#FF2800">The bonder is currently in building 346 Phoenex lab.</span>


The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.  
The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.  
[[Image:K-S 4524 wirebonder DTU.jpg|thumb|300px|K&S 4524 ball wire bonder]]
    
    
'''The user manual(s), user APV(s), technical information and contact information can be found in LabManager (requires login):'''  
'''The user manual(s), user APV(s), technical information and contact information can be found in LabManager (requires login):'''  

Revision as of 15:05, 9 August 2025

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

TPT HB100 Wire Bonder

Wire bonding is a method of making interconnections between a microchip and other electronics as part of semiconductor device fabrication. The TPT HB100 Wire Bonder was bought i 2025. It is an automatic desktop wire bonder and supports process guidance for the user. The bonder allows wedge- and ball-bonding, ribbon- and bump-bonding with one bond head.

The user manual(s), user APV(s), technical information and contact information can be found in LabManager (requires login):

TPT HB100 Wire Bonder

Ball Wire Bonder K&S 4524

K&S 4524 ball wire bonder

The bonder is currently in building 346 Phoenex lab.

The Ball Wire Bonder K&S 4524 is for high precision ball bonding. It is a semi-automatic wire bonder with good control of bond placement and bonding parameters.

The user manual(s), user APV(s), technical information and contact information can be found in LabManager (requires login):

Ball Wire Bonder

Equipment performance and process related parameters

Ball wire bond
Equipment TPT HB100 Wire Bonder Ball Wire Bonder
Purpose

THIS PART IS UNDER CONSTRUCTION

  • Al and Au 25µm wire bonding
  • Wedge and ball wire bonding
  • Au ribbon (100x20µm) bonding
    (we have tools and wire but it has not been tested)
  • Au 25µm wire bonding
  • Ball wire bonding
Performance
  • Manual operation
  • Wedge bonding:
    • recommended min. bonding area 200 µm x 200 µm
  • Ball bonding:
    • recommended min. bonding area 200 µm x 200 µm
    • recommended temperature 120 oC.
  • Semi-automatic and manual operation
  • Bond placement laser pointer
  • recommended min. bonding area 100 µm x 100 µm
  • recommended temperature 120 oC.
Substrates
  • Should be able to withstand the wire bonding temperature
  • Typical materials are: Alumina (Al2O3), AluminumNitride (AlN), std. circuit boards (FR4)