Specific Process Knowledge/Thin film deposition/Deposition of NbTi: Difference between revisions

Eves (talk | contribs)
Eves (talk | contribs)
Tag: Manual revert
Line 18: Line 18:
Users can deposit NbTi in either the Sputter-System (Lesker) or the Sputter-System Metal-Nitride(PC3) (Preferable option)
Users can deposit NbTi in either the Sputter-System (Lesker) or the Sputter-System Metal-Nitride(PC3) (Preferable option)


* [[Specific Process Knowledge/Thin film deposition/Deposition of NbTi/Deposition of NbTi in Sputter-System Metal-Nitride PC3|Deposition of NbTi in Sputter-System Metal-Nitride(PC3)]]
* [[Specific Process Knowledge/Thin film deposition/Deposition of NbTi/Deposition of NbTi in Sputter-System Metal-Nitride PC3/|Deposition of NbTi in Sputter-System Metal-Nitride(PC3)]]


==Comparison of sputter systems for alloy deposition==
==Comparison of sputter systems for alloy deposition==