Jump to content

Specific Process Knowledge/Thermal Process/RTP Jipelec 2: Difference between revisions

Pevo (talk | contribs)
Pevo (talk | contribs)
Line 142: Line 142:
|style="background:LightGrey; color:black"|
|style="background:LightGrey; color:black"|
* '''Max. 100 <sup>o</sup>C/s''' with '''carrier wafer''' or '''sample wafer'''
* '''Max. 100 <sup>o</sup>C/s''' with '''carrier wafer''' or '''sample wafer'''
* '''Max. 50 <sup>o</sup>C/s''' with SiC-coated graphite '''susceptor'''
* '''Max. 20 <sup>o</sup>C/s''' with SiC-coated graphite '''susceptor'''
|style="background:WhiteSmoke; color:black;" align="left"| At faster heating rates, the actual temperature might overshoot from the temperature setpoint in the recipe, and the susceptors/carriers might break.
|style="background:WhiteSmoke; color:black;" align="left"| At faster heating rates, the actual temperature might overshoot from the temperature setpoint in the recipe, and the susceptors/carriers might break.
|-
|-