Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4/Silicon Nitride Etch: Difference between revisions

From LabAdviser
Prakus (talk | contribs)
Prakus (talk | contribs)
No edit summary
Line 17: Line 17:
[[File:slowetch2_100% loadSRN_etchrate.png|400px|left|thumb|Note: etch rate for SRN with Slowetch 2. The wafers were processed on 4 different days,  the variation suggests process instability or chamber memory effects influencing etch behavior across runs.]]
[[File:slowetch2_100% loadSRN_etchrate.png|400px|left|thumb|Note: etch rate for SRN with Slowetch 2. The wafers were processed on 4 different days,  the variation suggests process instability or chamber memory effects influencing etch behavior across runs.]]
[[File:SRN_etch_rate_uniformity_nochambercondition.png|400px|left|thumb|Note: Compared to the first dataset (with chamber cleaning), the second set shows higher variability in etch performance despite identical recipes. Wafer 5, without conditioning, had the highest etch rate (11.5 nm/min) but poor uniformity, while Wafer 6 showed lower etch rate with improved uniformity. This confirms chamber conditioning significantly stabilizes SRN etch rates and enhances wafer-to-wafer uniformity.]]
[[File:SRN_etch_rate_uniformity_nochambercondition.png|400px|left|thumb|Note: Compared to the first dataset (with chamber cleaning), the second set shows higher variability in etch performance despite identical recipes. Wafer 5, without conditioning, had the highest etch rate (11.5 nm/min) but poor uniformity, while Wafer 6 showed lower etch rate with improved uniformity. This confirms chamber conditioning significantly stabilizes SRN etch rates and enhances wafer-to-wafer uniformity.]]
'''SRN (LPCVD) etch uniformity on 6″ wafer with ''Slowetch'' recipe'''
<br>
<br>
The process was repeated twice, but only one set of data is presented here.
The process was repeated twice, but only one set of data is presented here.
<br>
<br>

Revision as of 13:38, 28 July 2025

Feedback to this page: click here


THIS PAGE IS UNDER CONSTRUCTION

Etch rate uniformity & etch rate

SRN (LPCVD) etch uniformity on 6″ wafer with Slowetch 2 recipe


Process: No mask, 100 % load, etching was done after 10 mins chamber clean + 5 mins TDESC clean (for all wafers)
Note: etch rate for SRN with Slowetch 2. The wafers were processed on 4 different days, the variation suggests process instability or chamber memory effects influencing etch behavior across runs.
Note: Compared to the first dataset (with chamber cleaning), the second set shows higher variability in etch performance despite identical recipes. Wafer 5, without conditioning, had the highest etch rate (11.5 nm/min) but poor uniformity, while Wafer 6 showed lower etch rate with improved uniformity. This confirms chamber conditioning significantly stabilizes SRN etch rates and enhances wafer-to-wafer uniformity.

SRN (LPCVD) etch uniformity on 6″ wafer with Slowetch recipe


The process was repeated twice, but only one set of data is presented here.