Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of MoSi: Difference between revisions

From LabAdviser
Eves (talk | contribs)
Created page with "Molybdenum silicide is particularly attractive for optical coatings because co-sputtering Mo with Si allows precise control of MoSi stoichiometry—and, in turn, the film’s refractive index at the design wavelength. MoSi alloy can be deposited by DC co-sputtering in either Sputter-System Metal-Oxide (PC1) or Sputter-System Metal-Nitride (PC3)—collectively referred to as the Cluster Lesker. The process uses two 3-inch targets: *Mo (unbonded) *Si (indium-bonded) A..."
 
Eves (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_MoSi click here]'''
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i>
<br clear="all" />
== Deposition of MoSi ==
Molybdenum silicide is particularly attractive for optical coatings because co-sputtering Mo with Si allows precise control of MoSi stoichiometry—and, in turn, the film’s refractive index at the design wavelength.  
Molybdenum silicide is particularly attractive for optical coatings because co-sputtering Mo with Si allows precise control of MoSi stoichiometry—and, in turn, the film’s refractive index at the design wavelength.  



Revision as of 22:42, 16 July 2025

Feedback to this page: click here

Unless otherwise stated, this page is written by DTU Nanolab internal


Deposition of MoSi

Molybdenum silicide is particularly attractive for optical coatings because co-sputtering Mo with Si allows precise control of MoSi stoichiometry—and, in turn, the film’s refractive index at the design wavelength.

MoSi alloy can be deposited by DC co-sputtering in either Sputter-System Metal-Oxide (PC1) or Sputter-System Metal-Nitride (PC3)—collectively referred to as the Cluster Lesker. The process uses two 3-inch targets:

  • Mo (unbonded)
  • Si (indium-bonded)

Achieving the desired composition and optical properties requires careful tuning of three key parameters:

  • Magnetron power on each target
  • Substrate temperature
  • Deposition pressure

Below is a link summarizing process results obtained with the Metal-Oxide (PC1) system:

[Insert link]