Specific Process Knowledge/Polymer Processing: Difference between revisions
Appearance
| Line 16: | Line 16: | ||
* [[Specific_Process_Knowledge/Back-end_processing/Hot_Embosser|Hot Embossing]] (Compression Molding) | * [[Specific_Process_Knowledge/Back-end_processing/Hot_Embosser|Hot Embossing]] (Compression Molding) | ||
* [[Specific Process Knowledge/Back-end processing/Polymer Injection Molder|Injection Molding]] ''(not availabe at DTU Nanolab anymore (moved to DTU Mech))'' | * [[Specific Process Knowledge/Back-end processing/Polymer Injection Molder|Injection Molding]] ''(not availabe at DTU Nanolab anymore (moved to DTU Mech))'' | ||
* Polymer Casting (e.g. PDMS) | * Polymer Casting (e.g. [[Specific Process Knowledge/Characterization/Sample preparation| PDMS Casting]]) | ||
'''Specialized Processes:''' | '''Specialized Processes:''' | ||
* [[Specific Process Knowledge/Lithography/UVLithography|UV Lithography]] | * [[Specific Process Knowledge/Lithography/UVLithography|UV Lithography]] | ||
Revision as of 16:22, 10 June 2025
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
THIS PAGE IS UNDER CONSTRUCTION
Polymer Processing
There is a wide range of methods available to structure and modify polymers, though commonly done outside of a cleanroom.
Many polymer processing methods may require a mask or stamp or some kind, f.ex. injection molding, hot embossing or nano imprint lithography. Some methods can be used to directly "write" into the material, f.ex. laser ablation or micromilling. Other methods, like 3D printing or 2-photon polymerization are called additive methods as they create the structure by a building up the polymer structure.
Choose Method of Polymer Processing
- Nano Imprint Lithography
- Hot Embossing (Compression Molding)
- Injection Molding (not availabe at DTU Nanolab anymore (moved to DTU Mech))
- Polymer Casting (e.g. PDMS Casting)
Specialized Processes:
- UV Lithography
- Additive Techniques
- 3D printing
- 2-Photon Polymerization Lithography
- Plasma Etching
- FDTS coating (MVD)
- Laser Ablation
- Micro Milling (not generally availabe at DTU Nanolab)
- Extrusion Coating (not availabe at DTU Nanolab)
Choose Material for Polymer Processing
- Epoxy, e.g. SU-8
- Thermoplastic, e.g. PMMA, Topas (COC), PS, PC, PP, PET, etc
- Photo Resist, e.g. AZ resists