'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Lithium_niobate click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Lithium_niobate click here]''' | ||
==Etching of Lithium Niobate== | ==Etching of Lithium Niobate== | ||
*Etching af Lithium niobate is new to DTU Nanolab. There are some users doing it on the IBE and the ASE. We do not have any results we can show. | *Etching af Lithium niobate is new to DTU Nanolab. There are some users doing it on the IBE and the ASE. We do not have any results we can show. | ||