![[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE (Ionfab300+)]]
![[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE (Ionfab300+)]]
![[Specific_Process_Knowledge/Etch/ICP_Metal_Etcher|ICP metal]]
!
!
!
|-
|-
Line 33: Line 33:
!Generel description
!Generel description
|
|
|Sputtering of Ti - pure physical etch
|Sputtering of Lithium niobate - pure physical etch
|Dry plasma etch of Ti
|Dry plasma etch of Ti
|
|

Revision as of 14:29, 28 March 2025

THIS PAGE IS UNDER CONSTRUCTION

Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.

All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.

Feedback to this page: click here

Etching of Titanium

Etching of titanium can be done either by wet etch, dry etch or by sputtering with ions.


Comparison of Titanium Etch Methodes

IBE (Ionfab300+)
Generel description Sputtering of Lithium niobate - pure physical etch Dry plasma etch of Ti
Etch rate range
    • ~20nm/min
  • ~50-200 nm/min (depending on features size and etch load and recipe settings)
Etch profile
    • Anisotropic (angles sidewalls, typical around 70 dg)
  • Anisotropic (vertical sidewalls)
Substrate size

Smaller pieces glued to carrier wafer

  • #1 50mm wafer
  • #1 100mm wafer
  • #1 150mm wafer
  • #1 200mm wafer
  • smaller pieces on a carrier wafer
  • #1 100mm wafers (if you place it/bond it on a 150 mm carrier wafer)
  • #1 150mm wafers
Allowed materials
  • Silicon
  • Silicon oxides
  • Silicon nitrides
  • Lithium niobate
  • Metals from the +list
  • Metals from the -list
  • Alloys from the above list
  • Stainless steel
  • Glass
  • III-V materials
  • Resists
  • Polymers
  • Capton tape
  • And many more, please ask the Dryetch group
  • Silicon
  • Quartz/fused silica
  • Photoresist/e-beam resist
  • PolySilicon,
  • Silicon oxide
  • Silicon (oxy)nitride
  • Aluminium
  • Titanium
  • Chromium