==Getting a CIF file and exporting reference data to xy format from the ICSD==
==Getting a CIF file and exporting reference data to xy format from the ICSD==
On the ICSD main page you can run a query to find the available spectra for a given composition.  
On the ICSD main page you can run a query to find the available spectra for a given composition.  
A query will result in a list of entries that are more or less relevant. If possible choose the results with the "high quality data" marker. Remember to check that the data are recorded at a relevant temperature and pressure.
A query will result in a list of entries that are more or less relevant. If possible choose the results with the "high quality data" marker. Check that the data are recorded at a relevant temperature and pressure.


Once you have found a promising entry, click "Detailed View" and now you will see the reference data. At the top of the page you can click "CIF" and export a CIF file with all the information ready to import into the material database in SmartLab Studio II.
Once you have found a promising entry, click "Detailed View" and now you will see the reference data. At the top of the page you can click "CIF" and export a CIF file with all the information ready to import into the material database in SmartLab Studio II.