=== Data with HF generator=25W ===
=== Data with HF generator=25W ===
[[File:25W - thickness PECVD4 nitride QC.png|left|thumb|343x343px|Data from november to february of 15min QC nitride using 25W. The graph showcases thickness with standard error across time.]]
[[File:25W - thickness PECVD4 nitride QC.png|left|thumb|435x435px|Data from november to february of 15min QC nitride using 25W. The graph showcases thickness with standard error across time.]]
[[File:25W - Thickness filmtek vs ellipsometer.png|thumb|351x351px|Wafers had the thickness measured in both Filmtek and Ellipsometer, comparing the results.]]
[[File:25W - Thickness filmtek vs ellipsometer.png|thumb|436x436px|Wafers had the thickness measured in both Filmtek and Ellipsometer, comparing the results.]]
 
 
 
 
 
 
 
 
 
[[File:25W - refractive index QC nitride.png|left|thumb|435x435px|Data from november to february of 15min QC nitride using 25W. The graph showcases the refractive index with standard error across time.]]
[[File:25W - refractive index filmtek vs ellipsometer.png|thumb|436x436px|Wafers had the refractive index measured in both Filmtek and Ellipsometer, comparing the results.]]
 
 
 
 
 
 
 
 
 
 
 
 
 
[[File:25W - reflected power QC nitride.png|left|thumb|596x596px|Reflected power of different tests, whit 25W as the demanded power.]]
 
 
 
 




Line 19: Line 48:




[[File:25W - refractive index QC nitride.png|left|thumb|345x345px|Data from november to february of 15min QC nitride using 25W. The graph showcases the refractive index with standard error across time.]]
[[File:25W - refractive index filmtek vs ellipsometer.png|thumb|353x353px|Wafers had the refractive index measured in both Filmtek and Ellipsometer, comparing the results.]]


=== Data with HF generator=100W ===
=== Data with HF generator=100W ===
[[File:100W - thickness QC nitride.png|left|thumb|435x435px|Data from november to february of 15min QC nitride using 100W. The graph showcases thickness with standard error across time.]]