Descum of AZ 5214E on 100 mm wafers. The descum process development was done for a single substrate, as well as 3 substrates (for decreased ashing rate and improved ashing uniformity). The substrates were placed vertically in the glass boat.
Descum of AZ 5214E on 100 mm wafers. The descum process was tested for single substrates, as well as 3 substrates, placed vertically in the glass boat. For the 3 substrates only the center substrate was used for testing, the front and back wafers were used as dummy wafers.<br>


When running multiple wafers, the first and last wafers should always be dummy wafers.
For the 3 substrates only the center substrate was used for testing, the front and back wafers were used as dummy wafers. The wafers were placed in consecutive slots - when running multiple wafers in this way, the first and last wafers should always be dummy wafers.