'''Typical descum parameters'''
'''Typical descum parameters'''<br>
Tested with 1.5 µm AZ 5214E on 100 mm silicon substrate.
*O<sub>2</sub>: 100 sccm
*O<sub>2</sub>: 100 sccm
*N<sub>2</sub>: 100 sccm
*N<sub>2</sub>: 100 sccm