Upgrading the silicon etch capability at Danchip with the DRIE-Pegasus has pushed our old ASE (Advanced Silicon Etcher) out of the line so that it now only serves as backup silicon dry etcher. We have therefore decided that the ASE must be converted to a polymer etcher instead. Before releasing the tool for polymer etching it will have to be upgraded and all the 'old' silicon processes must be succesfully transfered to the new tool. We expect that this work will be completed towards mid 2011
= Polymer dry etching =
Upgrading the silicon etch capability at Danchip with the DRIE-Pegasus has pushed our old ASE (Advanced Silicon Etcher) out of the line so that it now only serves as backup silicon dry etcher. We have therefore decided that the ASE must be converted to a polymer etcher instead.  
 
%Before releasing the tool for polymer etching it will have to be upgraded and all the 'old' silicon processes must be succesfully transfered to the new tool. We expect that this work will be completed towards mid 2011


At the moment polymers can be etched in the plasma asher and to some extend in the RIE's. In RIE1 it is only for removing photo resist before or after a RIE etch if the plasma asher cannot be used for some reason. On RIE2 you can get allowance for some other polymer etching but you have to ask first.
At the moment polymers can be etched in the plasma asher and to some extend in the RIE's. In RIE1 it is only for removing photo resist before or after a RIE etch if the plasma asher cannot be used for some reason. On RIE2 you can get allowance for some other polymer etching but you have to ask first.


*[[Specific Process Knowledge/Etch/Etching of Polymer/Etch of Photo Resist using RIE|Etch of Photo Resist using RIE]]
*[[Specific Process Knowledge/Etch/Etching of Polymer/Etch of Photo Resist using RIE|Etch of Photo Resist using RIE]]

Revision as of 10:48, 8 August 2011

Polymer dry etching

Upgrading the silicon etch capability at Danchip with the DRIE-Pegasus has pushed our old ASE (Advanced Silicon Etcher) out of the line so that it now only serves as backup silicon dry etcher. We have therefore decided that the ASE must be converted to a polymer etcher instead.

%Before releasing the tool for polymer etching it will have to be upgraded and all the 'old' silicon processes must be succesfully transfered to the new tool. We expect that this work will be completed towards mid 2011

At the moment polymers can be etched in the plasma asher and to some extend in the RIE's. In RIE1 it is only for removing photo resist before or after a RIE etch if the plasma asher cannot be used for some reason. On RIE2 you can get allowance for some other polymer etching but you have to ask first.