Jump to content

Specific Process Knowledge/Lithography/EBeamLithography/AR-N 7520 New: Difference between revisions

Thope (talk | contribs)
Thope (talk | contribs)
Tag: Manual revert
Line 7: Line 7:
* Acceleration: 1000 RPM/s
* Acceleration: 1000 RPM/s
* Speed: 4000 RPM
* Speed: 4000 RPM
* Time: 90 s
* Time: 60 s
* Baking temperature: 85C
* Baking temperature: 85C
* Baking time: 60 s
* Baking time: 60 s