The single shot approach is illustrated in the center and right parts of the figure below as there are two ways to go about this. | The single shot approach is illustrated in the center and right parts of the figure below as there are two ways to go about this. | ||
*''' | *'''Single big box approach''': This approach is illustrated in the center of the figure below. The mask is a single box of the desired size of the array. The beam is then pitched with the SHOT x, n command where n determines the beam pitch and hence the pitch of the resulting circles. The size of the resulting circles is determined by the dwell time. | ||
*''' | *'''Array of small boxes approach''': This is illustrated on the right side of the figure. In this approach each circle is represented by a small 2x2 nm box, hence the pattern is an array of these small boxes and the beam pitch is set higher than the size of the box to produce a single beam shot in each box. Again, the size of the resulting circles is determined by the dwell time. | ||
{| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | {| style="border: none; border-spacing: 0; margin: 1em auto; text-align: center;" | ||