! Typical beam current [nA] !! Aperture !! Condition file
! Typical beam current [nA] !! Aperture !! Condition file
|-
| 0.12 || 4 || 0.12na_ap4
|-
| 0.16 || 4 || 0.16na_ap4
|-
|-
| 0.227 || 4 || 0.22na_ap4
| 0.227 || 4 || 0.22na_ap4
|-
| 0.4 || 4 || 0.4na_ap4
|-
| 0.5 || 4 || 0.5na_ap4
|-
| 0.815 || 4 || 0.8na_ap4
|}
|}