Line 21: Line 21:
Resulting resist thickness can be determined as y = ax<sup>b</sup>, where y is thickness [nm], x is spin speed [RPM], a = 11664 and b = -0.442.
Resulting resist thickness can be determined as y = ax<sup>b</sup>, where y is thickness [nm], x is spin speed [RPM], a = 11664 and b = -0.442.