==Oxidation==
==Oxidation==
At DTU Nanolab we have seven furnaces and one RTP (rapid thermal processor) for thermal oxidation of silicon samples: Boron Drive-in + Pre-dep furnace (A1), Gate Oxide furnace (A2), Phosphorous Drive-in furnace (A3), Anneal-oxide furnace (C1), Anneal-Bond furnace (C3), Al-Anneal furnace (C3) and Multipurpose Annealing furnace.
At DTU Nanolab we have seven furnaces and one RTP (rapid thermal processor) for thermal oxidation of silicon samples: Boron Drive-in + Pre-dep furnace (A1), Gate Oxide furnace (A2), Phosphorous Drive-in furnace (A3), Anneal-oxide furnace (C1), Anneal-Bond furnace (C3), Al-Anneal furnace (C3), Multipurpose Annealing furnace and Annealsys RTP.


Thermal oxidation can take place either by a dry process or by a wet process, depending on what furnace that is used for the oxidation. The film quality for a dry oxide is better than the film quality for a wet oxide with regards to density and dielectric constant. However, the oxidation rate is slow for dry oxidation.
Thermal oxidation can take place either by a dry process or by a wet process, depending on what furnace that is used for the oxidation. The film quality for a dry oxide is better than the film quality for a wet oxide with regards to density and dielectric constant. However, the oxidation rate is slow for dry oxidation.