At DTU Nanolab we have five furnaces and an RTP (Rapid thermal annealing) that can be used for annealing: Anneal-Oxide furnace (C1), Anneal-bond furnace (C3), Al_anneal furnace (C4), Multipurpose Anneal furnace and | At DTU Nanolab we have five furnaces and an RTP (Rapid thermal annealing) that can be used for annealing: Anneal-Oxide furnace (C1), Anneal-bond furnace (C3), Al_anneal furnace (C4), Multipurpose Anneal furnace and Jipelec2 RTP. Annealing normally takes place in an N<sub>2</sub> atmosphere, or it can be done in H<sub>2</sub> or a H<sub>2</sub>-N<sub>2</sub> gas mixture in the Multipurpose Anneal furnace. PECVD PBSG glass is annealed in a wet atmosphere which will also oxidize the silicon substrate. | ||
A 20 minutes N<sub>2</sub> annealing step is also included in all recipes on the oxidation furnace, this annealing is done after the oxidation. | A 20 minutes N<sub>2</sub> annealing step is also included in all recipes on the oxidation furnace, this annealing is done after the oxidation. | ||
Revision as of 14:56, 8 January 2024
Feedback to this page: click here
This page is written by DTU Nanolab internal
Annealing
At DTU Nanolab we have five furnaces and an RTP (Rapid thermal annealing) that can be used for annealing: Anneal-Oxide furnace (C1), Anneal-bond furnace (C3), Al_anneal furnace (C4), Multipurpose Anneal furnace and Jipelec2 RTP. Annealing normally takes place in an N2 atmosphere, or it can be done in H2 or a H2-N2 gas mixture in the Multipurpose Anneal furnace. PECVD PBSG glass is annealed in a wet atmosphere which will also oxidize the silicon substrate.
A 20 minutes N2 annealing step is also included in all recipes on the oxidation furnace, this annealing is done after the oxidation.
Comparison of the annealing furnaces
| General description | Annealing of 4" and 6" wafers. Annealing of wafers from the LPCVD furnaces and from PECVD4. | Annealing of wafers from Wafer Bonder 02 and from and PECVD4 and PECVD3. | Annealing of wafers with Al and ALD deposited AL2O3 and TiO2. | Rapid thermal processing, usually, annealing (RTA). | Annealing, oxidation and resist pyrolysis of different samples |
|---|---|---|---|---|---|
| Annealing gas |
|
|
|
|
|
| Process temperature |
|
|
|
|
|
| Substrate and Batch size |
|
|
|
|
|
| Allowed materials |
|
|
|
|
|