Jump to content

Specific Process Knowledge/Characterization/Drop Shape Analyzer: Difference between revisions

From LabAdviser
Rkch (talk | contribs)
Rkch (talk | contribs)
Line 11: Line 11:
'''The user manual, user APV(s), technical information, and contact information can be found in LabManager:'''  
'''The user manual, user APV(s), technical information, and contact information can be found in LabManager:'''  


[https://labmanager.dtu.dk/function.php?module=Machine&view=edit&id=520 Drop Shape Analyzer in LabManager]
[https://labmanager.dtu.dk/function.php?module=Machine&view=edit&id=520 Drop Shape Analyzer in LabManager]


==An overview of the performance of the Drop Shape Analyzer==
==An overview of the performance of the Drop Shape Analyzer==

Revision as of 15:54, 23 November 2023

Feedback to this page: click here

The Drop Shape Analyzer

The Krüss DSA 100s Drop Shape Analyzer in Cleanroom A-1

The Krüss DSA 100S Drop Shape Analyzer will analyze the shape of a drop of liquid on a surface, or suspended from a needle, in order to calculate the contact angle, or the surface tension, respectively. It is mostly used to determine the contact angle of water as a measure of the hydrophobicity/hydrophilicity of the sample surface.


The user manual, user APV(s), technical information, and contact information can be found in LabManager:

Drop Shape Analyzer in LabManager

An overview of the performance of the Drop Shape Analyzer

Purpose Imaging and analysis of of the shape of the interface between liquid and air
  • Measurement of contact angle between sample surface and liquid
  • Measurement of surface tension of liquid
Performance Measurement accuracy
  • Highly dependent on analysis conditions (image quality and fitting model) and method used; usually around ±0.5°. Using several measurement points is recommended.
Process parameters Available liquids
  • Syringe 1: Water (H2O)
  • Syringe 2: Diiodo-methane (CH2I2)
  • Syringe 3: Benzyl alcohol (C6H5CH2OH)
  • Syringe 4: Available
  • Manual dispense is also possible
Sample requirements Substrate material allowed
  • In principle all materials allowed in cleanroom
Substrate size
  • Up to 6" wafers. In order to measure, a few mm2 of flat surface is required.
Batch size
  • One sample at a time